Transactions of Nonferrous Metals Society of China (中国有色金属学报)2026DOI: 10.1016/S1003-6326(26)67065-3

Single Crystal NCM811 Cathode Material Prepared by Rapid Solvothermal Method

Polycrystalline LiNi0.8Co0.1Mn0.1O2 (NCM811) cathodes undergo intergranular cracking and structural collapse during extended cycling, limiting their commercial viability. This study reports single-crystalline NCM811 synthesized via a rapid ethanol–water solvothermal method. The solvothermal duration was varied, and the 60 min sample (NCM-60) exhibited optimal electrochemical performance. X-ray diffractometry confirmed an α-NaFeO2 structure with R-3m space group and high crystallinity. NCM-60 delivered a reversible capacity of 157.28 mA·h/g at 1C and a capacity retention of 55.06% after 200 cycles, significantly outperforming polycrystalline NCM (PC-NCM). Cross-sectional scanning electron microscopy revealed no apparent cracks in NCM-60 after 200 cycles, whereas PC-NCM exhibited severe intergranular fracture. The results demonstrate that shortening solvothermal time reduces precursor particle size and crystallinity, but 60 min yields the best balance. Pre-oxidation of the carbonate precursor before lithiation is recommended to mitigate CO2 evolution and lithium–nickel disorder during high-temperature sintering. This rapid solvothermal route offers a scalable pathway to single-crystal NCM811 with enhanced cycling stability and mechanical integrity.