Transactions of Nonferrous Metals Society of China (中国有色金属学报)2026DOI: 10.1016/S1003-6326(26)67062-8

Adjusting mechanisms for ultrafine-grained microstructures during hot deformation of Ni−38Cr−3.8Al alloy via pre-ageing precipitation

The influence of pre-ageing temperature on dynamic recrystallization (DRX) and microstructure evolution during hot compression of Ni−38Cr−3.8Al alloy was investigated. Five samples with varying pre-precipitation states were fabricated. Pre-ageing treatment precipitates α-Cr phases in lamellar and particle forms. During subsequent hot deformation, pre-precipitated α-Cr lamellae undergo dissolution fragmentation and spheroidization, transforming into finer particles due to elevated temperature and high-density dislocations. At 560 °C, an incomplete discontinuous precipitation (DP) state restrains DRX, producing necklace-like microstructures. Above 640 °C, a complete DP state with fully lamellar structures promotes DRX, yielding ultrafine-grained (UFG) microstructures. Coarse α-Cr particles enhance DRX through particle-stimulated nucleation (PSN) and discontinuous DRX mechanisms, while dissolved α-Cr lamellae promote DRX via continuous DRX. DRX kinetics analysis indicates that increasing pre-ageing temperature accelerates DRX, evidenced by reduced critical strain and peak strain, and increased DRX volume fraction. To achieve UFG microstructures during hot deformation, fully lamellar structures should be precipitated during pre-ageing. These findings provide a processing pathway for tailoring microstructures in high-Cr nickel-based alloys.

Transactions of Nonferrous Metals Society of China (中国有色金属学报)2025DOI: 10.1016/S1003-6326(25)67030-0

Realizing stable zinc anodes via three-dimensional passivation layer

A porous three-dimensional (3D) structure was created on the Zn surface by an electrostripping activation process under high current density, which could suppress the non-uniform Zn2+ deposition induced by the “tip effect.” Moreover, a functional CeO4H4/Ce(OH)3 passivation layer was introduced to prevent electrochemical corrosion and facilitate electrolyte infiltration. Benefiting from the ingenious 3D structure and passivation layer, the assembled symmetric cell delivers a long lifespan of over 1500 h at 5 mA/cm2. Even at 20 mA/cm2, the electrode can still operate for over 300 h. The R-Zn@CeǁMnO2 full cell exhibits a capacity of 205.3 mA·h/g after 300 cycles at a current density of 0.3 A/g.